Mixing: pour the additive into a container according to the proportion, then slowly pour the powder into the additive, and at the same time fully stir until the caking is uniform, and let it stand for 5 minutes before use; Intermittent stirring should be maintained during use to prevent layered precipitation.
Mixing ratio: liquid (additive): powder = 1: 2.5-2.77 (weight ratio)
Construction: evenly brush or spray the mixed slurry on the wet substrate with a hard brush, roller or shotcrete machine; If it is used for moisture protection, only one layer is needed; If it is waterproof, it needs two or three coats. When the first layer is dry enough not to stick to hands (usually 1-2 hours), the second layer can be painted, and the painting directions of every two layers should intersect vertically.
Coating protection: after the slurry construction is completed, the coating must be protected before it is completely dried, including no pedestrians, rain washing, exposure to the sun, sharp instrument damage, etc. Completely dry
The coating does not need to be a special protective layer.
Coating curing: It is recommended to cover the coating with wet cloth or spray water to cure the coating after 24 hours of coating construction, generally 2-3 days; In places with high air humidity and poor ventilation, the drying and curing time will be longer, otherwise, in the environment with poor air circulation, mechanical ventilation can be used to speed up the drying and curing speed, which is beneficial to the project progress.
Construction temperature: suitable for use in the environment of 5℃-40℃. Packaging: (25kg powder +9kg additive)/set.
(14.5kg powder +5.5kg additive)/set.
(7 kg powder +3 kg additive)/set
Appearance: liquid material: milky white toner material: gray
Stored in a dry and cool place, the shelf life of unopened products is 12 months.
Product quality assurance
The product conforms to the application technical index, and the quality is reliable and stable, and it bears the responsibility of defective products. Before construction, it is recommended to read the instructions carefully and carry out the construction as required.